Essentials of Dentistry. 2024;3(1):15-21.
ABSTRACT
Background: Evaluating the prolonged efficacy of restorative materials hinges significantly on their ability to resist discoloration. This study aims to assess the discoloration resistance of computer-aided design/computer-aided manufacturing restorative materials featuring distinct chemical compositions.
Methods: A1-colored samples from 4 diverse CAD/CAM restorative materials (Lava Ultimate, Tetric CAD, Vita Enamic, and IPS e.max CAD), each with a 2 mm thickness (n = 12), were meticulously prepared. Baseline CIE L*a*b* values were measured using a spectrophotometer, and randomly assigned samples were subjected to a 28-day immersion in either distilled water (control group) or coffee (n = 6). After the designated period, CIE L*a*b* values were reevaluated, and ΔEab values were computed. A 2-way analysis of variance test was employed to scrutinize the influence of both the restorative material type and solution type on quantitative variables (P < .05).
Results: In the comparison of samples immersed in coffee, IPS e.max CAD demonstrated significantly less staining than other samples, while Lava Ultimate exhibited significantly more staining (P < .05). No significant difference in ΔEab was observed among CAD/CAM restorative materials kept in distilled water. Although the ΔEab values of specimens immersed in distilled water remained below the CIELAB 50:50% acceptability threshold (ΔEab = 2.7), samples immersed in coffee exceeded this threshold.
Conclusion: The resistance to discoloration is influenced by both the restorative material and the nature of the solution. Consequently, clinicians may opt for restorative materials displaying heightened discoloration resistance or provide comprehensive guidance to patients regarding staining beverages and effective oral hygiene practices.
KEYWORDS
Computer-aided design/computer-aided manufacturing · color stability · discoloration · resin-matrix ceramics
STUDY SUMMARY
This in vitro study compared the discoloration resistance of four CAD/CAM restorative materials after 28 days of immersion in coffee or distilled water, measured with a spectrophotometer against the CIELAB acceptability threshold. In coffee, the lithium disilicate glass-ceramic stained significantly less and the resin nanoceramic significantly more than the other materials, while no significant differences appeared between materials stored in water. Color change stayed below the acceptability threshold in water and exceeded it in coffee for all materials tested.